1. Home
  2. Main Catalog

Hardcarb Products

  • Available forms
  • Hardness
  • Major hard-phase(s)
  • Suitability - Abrasion
  • Suitability - Corrosion
  • Suitability - Erosion
  • Suitability - Impact
  • Suitability - Temperature
    • EN 14700 alloy category: Fe 10
    • Available forms: welding electrodes, cored wires
    • Major alloying elements: Cr, Ni, Mn, Fe
    • Major hard-phase(s): None
    • Hardness as per DIN 32525-4: 180 - 200 HB (as welded) | 330 - 370 HB (work hardened)
    • Service temperature: 300 ᵒC
    • Weld deposit density: ~ 8 g/cc
    5.6
    • EN 14700 alloy category: ISO 1071: E C NiCu-B
    • Available forms: welding electrodes
    • Major alloying elements: C, Si, Mn, Ni, Cu, Fe
    • Major hard-phase(s): -
    • Hardness as per DIN 32525-4: approx. 170 HB
    • Service temperature: -
    • Weld deposit density: ~ 8.20 g/cc
    • EN 14700 alloy category: ISO 1071: E C Ni-CI 1
    • Available forms: welding electrodes
    • Major alloying elements: C, Si, Mn, Ni, Cu, Fe
    • Major hard-phase(s): -
    • Hardness as per DIN 32525-4: approx. 170 HB
    • Service temperature: -
    • Weld deposit density: ~ 8 g/cc
    • EN 14700 alloy category: ISO 1071: E C Ni-CI 1
    • Available forms: welding electrodes
    • Major alloying elements: C, Si, Mn, Ni, Cu, Fe
    • Major hard-phase(s): -
    • Hardness as per DIN 32525-4: approx. 160 HB
    • Service temperature: -
    • Weld deposit density: ~ 8 g/cc
    • EN 14700 alloy category: ISO 1071: E C Ni-CI 1
    • Available forms: welding electrodes
    • Major alloying elements: C, Si, Mn, Ni, Cu, Fe
    • Major hard-phase(s): -
    • Hardness as per DIN 32525-4: approx. 160 HB
    • Service temperature: -
    • Weld deposit density: ~ 8 g/cc
    • EN 14700 alloy category: ISO 1071: E C NiFe-1 1
    • Available forms: welding electrodes
    • Major alloying elements: C, Si, Mn, Ni, Fe
    • Major hard-phase(s): -
    • Hardness as per DIN 32525-4: approx. 190 HB
    • Service temperature: -
    • Weld deposit density: ~ 8 g/cc
    • EN 14700 alloy category: ISO 1071: E C NiFe-1 1
    • Available forms: welding electrodes
    • Major alloying elements: C, Si, Mn, Ni, Cu, Fe
    • Major hard-phase(s): -
    • Hardness as per DIN 32525-4: approx. 190 HB
    • Service temperature: -
    • Weld deposit density: ~ 8 g/cc
    • EN 14700 alloy category: ISO 1071: E C NiFe-1 1
    • Available forms: welding electrodes, cored wires
    • Major alloying elements: C, Si, Mn, Ni, Cu, Fe
    • Major hard-phase(s): -
    • Hardness as per DIN 32525-4: approx. 170 HB
    • Service temperature: -
    • Weld deposit density: ~ 8 g/cc
    • EN 14700 alloy category: ISO 1071: E C NiFe-1 1
    • Available forms: welding electrodes
    • Major alloying elements: C, Si, Mn, Ni, Cu, Fe
    • Major hard-phase(s): -
    • Hardness as per DIN 32525-4: approx. 170 HB
    • Service temperature: -
    • Weld deposit density: ~ 8 g/cc
    • EN 14700 alloy category: ISO 1071: E C FeC - GF 1
    • Available forms: welding electrodes
    • Major alloying elements: C, Si, Mn, Ti, Fe
    • Major hard-phase(s): -
    • Hardness as per DIN 32525-4: approx. 350 HB (as welded) approx. 54 HRC (one layer on cast iron)
    • Service temperature: -
    • Weld deposit density: ~ 8 g/cc
    • EN 14700 alloy category: AWS A5.11: ENiCrFe-3
    • Available forms: welding electrodes
    • Major alloying elements: C, Mn, Cr, Mo, Nb, Fe, Ni
    • Major hard-phase(s): -
    • Hardness as per DIN 32525-4: 180 - 200 HB (as welded) 330 - 370 HB (work hardened)
    • Service temperature: -269 °C up to above 550 °C
    • Weld deposit density: ~ 8 g/cc
    • EN 14700 alloy category: AWS A5.11: ENiCrFe-2 / mod.
    • Available forms: welding electrodes
    • Major alloying elements: C, Mn, Cr, Mo, Nb, Fe, Ni
    • Major hard-phase(s): -
    • Hardness as per DIN 32525-4: 180 - 200 HB (as welded) 330 - 370 HB (work hardened)
    • Service temperature: -196 °C up to 550 °C
    • Weld deposit density: ~ 8 g/cc
1 2 3 4 7 8 9