Tungsten carbide base superalloys

  • Available forms
  • Hardness
  • Major hard-phase(s)
  • Suitability - Abrasion
  • Suitability - Corrosion
  • Suitability - Erosion
  • Suitability - Impact
  • Suitability - Temperature
    • EN 14700 alloy category: Ni 20
    • Available forms: welding electrodes (flexible rope)
    • Major alloying elements: Spherical Fused Tungsten Carbide, NiCrBSi
    • Major hard-phase(s): Spherical Fused Tungsten Carbides
    • Hardness as per DIN 32525-4: 50 - 65 HRC / 515 - 825 HV
    • Service temperature: 500 C
    • Weld deposit density: ~ 13.65 g/cc
    8.6
    • EN 14700 alloy category: Ni 20
    • Available forms: welding electrodes (flexible rope)
    • Major alloying elements: Spherical Fused Tungsten Carbide, NiCrBSi
    • Major hard-phase(s): Spherical Fused Tungsten Carbides
    • Hardness as per DIN 32525-4: 50 - 65 HRC / 515 - 825 HV
    • Service temperature: 500 C
    • Weld deposit density: ~ 13.10 g/cc
    • EN 14700 alloy category: Ni 20
    • Available forms: Cored wires
    • Major alloying elements: Spherical fused tungsten carbides, NiCrBSi
    • Major hard-phase(s): spherical fused tungsten carbides
    • Hardness as per DIN 32525-4: 66 - 69 HRC / 865 - 1050 HV
    • Service temperature: 500 C
    • Weld deposit density: ~ 12 - 13 g/cc
    7.4
    • EN 14700 alloy category: Fe 20
    • Available forms: Welding electrodes
    • Major alloying elements: Spherical Fused Tungsten Carbides, Fe matrix
    • Major hard-phase(s): Spherical Fused Tungsten Carbides
    • Hardness as per DIN 32525-4: 60 - 66 HRC / 700 - 865 HV
    • Service temperature: 500 C
    • Weld deposit density: ~ 13.10 g/cc
    5.8
    • EN 14700 alloy category: Fe 20
    • Available forms: Welding electrodes (Pre-alloyed tube)
    • Major alloying elements: Spherical Fused Tungsten Carbides, Fe matrix
    • Major hard-phase(s): Spherical Fused Tungsten Carbides
    • Hardness as per DIN 32525-4: 55 - 60 HRC / 590 - 700 HV
    • Service temperature: 500 C
    • Weld deposit density: ~ 13.10 g/cc
    6.0
    • EN 14700 alloy category: Ni 20
    • Available forms: welding electrodes (flexible rope)
    • Major alloying elements: Fused Tungsten Carbides, NiCrBSi
    • Major hard-phase(s): Fused Tungsten Carbides
    • Hardness as per DIN 32525-4: 50 - 65 HRC / 515 - 825 HV
    • Service temperature: 500 C
    • Weld deposit density: ~ 13.65 g/cc
    8.4
    • EN 14700 alloy category: Ni 20
    • Available forms: welding electrodes (flexible rope)
    • Major alloying elements: Fused Tungsten Carbides, NiCrBSi
    • Major hard-phase(s): Fused Tungsten Carbides
    • Hardness as per DIN 32525-4: 50 - 65 HRC / 515 - 825 HV
    • Service temperature: 500 C
    • Weld deposit density: ~ 13.65 g/cc
    • EN 14700 alloy category: Fe 20
    • Available forms: Welding electrodes (Tubular electrode)
    • Major alloying elements: WSC / FTC, Cr3C2, Fe
    • Major hard-phase(s): Fused Tungsten carbides, Chromium carbides
    • Hardness as per DIN 32525-4: 64 - 68 HRC / 900 - 1100 HV
    • Service temperature: 500 C
    • Weld deposit density: ~ 12 .40 g/cc
    5.4
    • EN 14700 alloy category: Non-standard special material
    • Available forms: Welding electrodes (composite rod)
    • Major alloying elements: Cemented Tungsten Carbide, Cu-Ni-Zn matrix
    • Major hard-phase(s): Cemented Tungsten Carbide
    • Hardness as per DIN 32525-4: 1300 HV to 1600 HV (Carbide Hardness)
    • Service temperature: 500 C
    • Weld deposit density: ~ 12.20 g/cc
    6.2
    • EN 14700 alloy category: Ni 20
    • Available forms: Cored wire
    • Major alloying elements: Fused Tungsten Carbides, NiCrBSi
    • Major hard-phase(s): Fused Tungsten Carbides
    • Hardness as per DIN 32525-4: 66 - 69 HRC / 865 - 1050 HV
    • Service temperature: 500 C
    • Weld deposit density: ~ 12 - 13 g/cc
    7.4
    • EN 14700 alloy category: Fe 20
    • Available forms: Cored wires
    • Major alloying elements: Fused Tungsten Carbides, Fe matrix
    • Major hard-phase(s): Fused Tungsten Carbides
    • Hardness as per DIN 32525-4: 66 - 69 HRC / 865 - 1050 HV
    • Service temperature: 500 C
    • Weld deposit density: ~ 12 - 13 g/cc
    6.0
    • EN 14700 alloy category: Fe 20
    • Available forms: welding electrodes
    • Major alloying elements: Fused Tungsten Carbides, Fe matrix
    • Major hard-phase(s): Fused Tungsten Carbides
    • Hardness as per DIN 32525-4: 60 - 66 HRC / 700 - 865 HV
    • Service temperature: 500 C
    • Weld deposit density: ~ 13.10 g/cc
    5.8