- Home
- Main Catalog
- Superalloy Hardfacing
- Tungsten carbide base superalloys
Tungsten carbide base superalloys
Name (A-Z)
Tungsten carbide base superalloys
- Buffer layers - Build up - Cladding - Joining
- Cast iron
- Dissimilar & stainless steels
- Manganese steel
- Metal-to-Earth wear
- High impact, high abrasion
- High stress, high abrasion
- Overalloyed solutions
- Severe abrasion
- Severe abrasion with corrosion
- Severe abrasion with erosion
- Severe abrasion with erosion, temperature
- Severe impact
- Metal-to-Metal wear
- Cold wear
- Hot wear (tool steel)
- Hot wear with corrosion & thermal fatigue
- Superalloy Hardfacing
- Cobalt base superalloys
- Iron base superalloys
- Nickel base superalloys
Available forms
Hardness
Major hard-phase(s)
Suitability - Abrasion
Suitability - Corrosion
Suitability - Erosion
Suitability - Impact
Suitability - Temperature
- EN 14700 alloy category: Fe 20
- Available forms: Welding electrodes (Pre-alloyed tube)
- Major alloying elements: Fused Tungsten Carbides, Fe matrix
- Major hard-phase(s): Fused Tungsten Carbides
- Hardness as per DIN 32525-4: 55 - 60 HRC / 590 - 700 HV
- Service temperature: 500 C
- Weld deposit density: ~ 13.10 g/cc
- View Details →
- EN 14700 alloy category: Fe 20
- Available forms: welding electrodes
- Major alloying elements: Fused Tungsten Carbides, Fe matrix
- Major hard-phase(s): Fused Tungsten Carbides
- Hardness as per DIN 32525-4: 60 - 66 HRC / 700 - 865 HV
- Service temperature: 500 C
- Weld deposit density: ~ 13.10 g/cc
- View Details →
- EN 14700 alloy category: Fe 20
- Available forms: Cored wires
- Major alloying elements: Fused Tungsten Carbides, Fe matrix
- Major hard-phase(s): Fused Tungsten Carbides
- Hardness as per DIN 32525-4: 66 - 69 HRC / 865 - 1050 HV
- Service temperature: 500 C
- Weld deposit density: ~ 12 - 13 g/cc
- View Details →
- EN 14700 alloy category: Ni 20
- Available forms: Cored wire
- Major alloying elements: Fused Tungsten Carbides, NiCrBSi
- Major hard-phase(s): Fused Tungsten Carbides
- Hardness as per DIN 32525-4: 66 - 69 HRC / 865 - 1050 HV
- Service temperature: 500 C
- Weld deposit density: ~ 12 - 13 g/cc
- View Details →
- EN 14700 alloy category: Non-standard special material
- Available forms: Welding electrodes (composite rod)
- Major alloying elements: Cemented Tungsten Carbide, Cu-Ni-Zn matrix
- Major hard-phase(s): Cemented Tungsten Carbide
- Hardness as per DIN 32525-4: 1300 HV to 1600 HV (Carbide Hardness)
- Service temperature: 500 C
- Weld deposit density: ~ 12.20 g/cc
- View Details →
- EN 14700 alloy category: Fe 20
- Available forms: Welding electrodes (Tubular electrode)
- Major alloying elements: WSC / FTC, Cr3C2, Fe
- Major hard-phase(s): Fused Tungsten carbides, Chromium carbides
- Hardness as per DIN 32525-4: 64 - 68 HRC / 900 - 1100 HV
- Service temperature: 500 C
- Weld deposit density: ~ 12 .40 g/cc
- View Details →
- EN 14700 alloy category: Ni 20
- Available forms: welding electrodes (flexible rope)
- Major alloying elements: Fused Tungsten Carbides, NiCrBSi
- Major hard-phase(s): Fused Tungsten Carbides
- Hardness as per DIN 32525-4: 50 - 65 HRC / 515 - 825 HV
- Service temperature: 500 C
- Weld deposit density: ~ 13.65 g/cc
- View Details →
- EN 14700 alloy category: Ni 20
- Available forms: welding electrodes (flexible rope)
- Major alloying elements: Fused Tungsten Carbides, NiCrBSi
- Major hard-phase(s): Fused Tungsten Carbides
- Hardness as per DIN 32525-4: 50 - 65 HRC / 515 - 825 HV
- Service temperature: 500 C
- Weld deposit density: ~ 13.65 g/cc
- View Details →
- EN 14700 alloy category: Fe 20
- Available forms: Welding electrodes (Pre-alloyed tube)
- Major alloying elements: Spherical Fused Tungsten Carbides, Fe matrix
- Major hard-phase(s): Spherical Fused Tungsten Carbides
- Hardness as per DIN 32525-4: 55 - 60 HRC / 590 - 700 HV
- Service temperature: 500 C
- Weld deposit density: ~ 13.10 g/cc
- View Details →
- EN 14700 alloy category: Fe 20
- Available forms: Welding electrodes
- Major alloying elements: Spherical Fused Tungsten Carbides, Fe matrix
- Major hard-phase(s): Spherical Fused Tungsten Carbides
- Hardness as per DIN 32525-4: 60 - 66 HRC / 700 - 865 HV
- Service temperature: 500 C
- Weld deposit density: ~ 13.10 g/cc
- View Details →
- EN 14700 alloy category: Ni 20
- Available forms: Cored wires
- Major alloying elements: Spherical fused tungsten carbides, NiCrBSi
- Major hard-phase(s): spherical fused tungsten carbides
- Hardness as per DIN 32525-4: 66 - 69 HRC / 865 - 1050 HV
- Service temperature: 500 C
- Weld deposit density: ~ 12 - 13 g/cc
- View Details →
- EN 14700 alloy category: Ni 20
- Available forms: welding electrodes (flexible rope)
- Major alloying elements: Spherical Fused Tungsten Carbide, NiCrBSi
- Major hard-phase(s): Spherical Fused Tungsten Carbides
- Hardness as per DIN 32525-4: 50 - 65 HRC / 515 - 825 HV
- Service temperature: 500 C
- Weld deposit density: ~ 13.10 g/cc
- View Details →