    • EN 14700 alloy category: Fe 20
    • Available forms: Welding electrodes (Pre-alloyed tube)
    • Major alloying elements: Fused Tungsten Carbides, Fe matrix
    • Major hard-phase(s): Fused Tungsten Carbides
    • Hardness as per DIN 32525-4: 55 - 60 HRC / 590 - 700 HV
    • Service temperature: 500 C
    • Weld deposit density: ~ 13.10 g/cc