Superalloy Hardfacing
- Buffer layers - Build up - Cladding - Joining
- Cast iron
- Dissimilar & stainless steels
- Manganese steel
- Metal-to-Earth wear
- High impact, high abrasion
- High stress, high abrasion
- Overalloyed solutions
- Severe abrasion
- Severe abrasion with corrosion
- Severe abrasion with erosion
- Severe abrasion with erosion, temperature
- Severe impact
- Metal-to-Metal wear
- Cold wear
- Hot wear (tool steel)
- Hot wear with corrosion & thermal fatigue
- Cobalt base superalloys
- Iron base superalloys
- Nickel base superalloys
- Tungsten carbide base superalloys
Available forms
Hardness
Major hard-phase(s)
Suitability - Abrasion
Suitability - Corrosion
Suitability - Erosion
Suitability - Impact
Suitability - Temperature
Sub Categories
- Cobalt base superalloys
- Iron base superalloys
- Nickel base superalloys
- Tungsten carbide base superalloys
- EN 14700 alloy category: Fe 20
- Available forms: Welding electrodes (Pre-alloyed tube)
- Major alloying elements: Fused Tungsten Carbides, Fe matrix
- Major hard-phase(s): Fused Tungsten Carbides
- Hardness as per DIN 32525-4: 55 - 60 HRC / 590 - 700 HV
- Service temperature: 500 C
- Weld deposit density: ~ 13.10 g/cc
- View Details →
- EN 14700 alloy category: Ni3
- Available forms: Atomized powders (Fuseweld - Powder welding)
- Major alloying elements: C, Cr, B, Si, Fe, Ni
- Major hard-phase(s): Fine metallic borides
- Hardness as per DIN 32525-4: 56 - 63 HRC
- Service temperature: 650 C
- Weld deposit density: ~ 7.80 g/cc
- View Details →
- EN 14700 alloy category: Ni3
- Available forms: Bare rods, cored wires, atomized powders
- Major alloying elements: C, Cr, B, Si, Fe, Ni
- Major hard-phase(s): Fine metallic borides
- Hardness as per DIN 32525-4: 56 - 63 HRC
- Service temperature: 650 C
- Weld deposit density: ~ 7.80 g/cc
- View Details →
- EN 14700 alloy category: Ni3
- Available forms: Atomized powders (Fuseweld - Powder welding)
- Major alloying elements: C, Cr, B, Si, Fe, Ni
- Major hard-phase(s): Fine metallic borides
- Hardness as per DIN 32525-4: 39 - 43 HRC
- Service temperature: 650 C
- Weld deposit density: ~ 8.20 g/cc
- View Details →
- EN 14700 alloy category: Ni3
- Available forms: Bare rods, cored wires, atomized powders
- Major alloying elements: C, Cr, B, Si, Fe, Ni
- Major hard-phase(s): Fine metallic borides
- Hardness as per DIN 32525-4: 35 - 40 HRC
- Service temperature: 650 C
- Weld deposit density: ~ 8.20 g/cc
- View Details →
- EN 14700 alloy category: Co1
- Available forms: Bare rods, welding electrodes, cored wires, atomized powders
- Major alloying elements: C, Si, Mn, Cr, Ni, W, Mo, Fe, Co
- Major hard-phase(s): -
- Hardness as per DIN 32525-4: 29 - 40 HRC / 290 - 430 HV
- Service temperature: 700 C
- Weld deposit density: ~ 8.33 g/cc
- View Details →
- EN 14700 alloy category: Co2
- Available forms: Bare rods, welding electrodes, cored wires, atomized powders
- Major alloying elements: C, Si, Mn, Cr, Ni, W, Mo, Fe, Co
- Major hard-phase(s): CrW carbides
- Hardness as per DIN 32525-4: 46 - 51 HRC / 450 - 540 HV
- Service temperature: 700 C
- Weld deposit density: ~ 8.50 g/cc
- View Details →
- EN 14700 alloy category: Co2
- Available forms: Bare rods, welding electrodes, cored wires, atomized powders
- Major alloying elements: C, Si, Mn, Cr, Ni, W, Mo, Fe, Co
- Major hard-phase(s): CrW carbides
- Hardness as per DIN 32525-4: 40 - 45 HRC / 390 - 450 HV
- Service temperature: 600 C
- Weld deposit density: ~ 8.44 g/cc
- View Details →
- EN 14700 alloy category: Co3
- Available forms: Bare rods, welding electrodes, cored wires, atomized powders
- Major alloying elements: C, Si, Mn, Cr, Ni, W, Mo, Fe, Co
- Major hard-phase(s): CrW carbides
- Hardness as per DIN 32525-4: 53 - 57 HRC / 550 - 650 HV
- Service temperature: 800 C
- Weld deposit density: ~ 8.7 g/cc
- View Details →
- EN 14700 alloy category: Fe 16 gtz
- Available forms: welding electrodes, cored wires, composite wearplates
- Major alloying elements: C, Si, Mn, Cr, Nb, Mo, W, B, Fe
- Major hard-phase(s): Metallic carbo-borides
- Hardness as per DIN 32525-4: 69 - 72 HRC / 1000 - 1200 HV
- Service temperature: 900 C
- Weld deposit density: ~ 8.60 g/cc
- View Details →
- EN 14700 alloy category: Fe 16 gtz
- Available forms: welding electrodes, cored wires, composite wearplates
- Major alloying elements: C, Si, Mn, Cr, Nb, Mo, W, B, Fe
- Major hard-phase(s): Metallic carbo-borides
- Hardness as per DIN 32525-4: 69 - 72 HRC / 1000 - 1200 HV
- Service temperature: 900 C
- Weld deposit density: ~ 8.50 g/cc
- View Details →
- EN 14700 alloy category: Fe 16 gtz
- Available forms: welding electrodes, cored wires, composite wearplates
- Major alloying elements: C, Si, Mn, Cr, Nb, Mo, B, Fe
- Major hard-phase(s): Metallic carbo-borides
- Hardness as per DIN 32525-4: 67 - 72 HRC / 900 - 1200 HV
- Service temperature: 850 C
- Weld deposit density: ~ 7.6 g/cc
- View Details →