- Home
- Main Catalog
- Buffer layers - Build up - Cladding - Joining
- Dissimilar & stainless steels
Dissimilar & stainless steels
Date (default)
Dissimilar & stainless steels
- Buffer layers - Build up - Cladding - Joining
- Cast iron
- Manganese steel
- Metal-to-Earth wear
- High impact, high abrasion
- High stress, high abrasion
- Overalloyed solutions
- Severe abrasion
- Severe abrasion with corrosion
- Severe abrasion with erosion
- Severe abrasion with erosion, temperature
- Severe impact
- Metal-to-Metal wear
- Cold wear
- Hot wear (tool steel)
- Hot wear with corrosion & thermal fatigue
- Superalloy Hardfacing
- Cobalt base superalloys
- Iron base superalloys
- Nickel base superalloys
- Tungsten carbide base superalloys
Available forms
Hardness
Major hard-phase(s)
Suitability - Abrasion
Suitability - Corrosion
Suitability - Erosion
Suitability - Impact
Suitability - Temperature
- EN 14700 alloy category: Fe 10
- Available forms: welding electrodes, cored wires
- Major alloying elements: Cr, Ni, Mn, Fe
- Major hard-phase(s): None
- Hardness as per DIN 32525-4: 180 - 200 HB (as welded) | 330 - 370 HB (work hardened)
- Service temperature: 300 ᵒC
- Weld deposit density: ~ 8 g/cc
- View Details →
- EN 14700 alloy category: AWS A5.11: ENiCrFe-3
- Available forms: welding electrodes
- Major alloying elements: C, Mn, Cr, Mo, Nb, Fe, Ni
- Major hard-phase(s): -
- Hardness as per DIN 32525-4: 180 - 200 HB (as welded) 330 - 370 HB (work hardened)
- Service temperature: -269 °C up to above 550 °C
- Weld deposit density: ~ 8 g/cc
- View Details →
- EN 14700 alloy category: AWS A5.11: ENiCrFe-2 / mod.
- Available forms: welding electrodes
- Major alloying elements: C, Mn, Cr, Mo, Nb, Fe, Ni
- Major hard-phase(s): -
- Hardness as per DIN 32525-4: 180 - 200 HB (as welded) 330 - 370 HB (work hardened)
- Service temperature: -196 °C up to 550 °C
- Weld deposit density: ~ 8 g/cc
- View Details →
- EN 14700 alloy category: Fe 11
- Available forms: welding electrodes, cored wires
- Major alloying elements: C ,Si, Cr, Ni, Mn, Fe
- Major hard-phase(s): -
- Hardness as per DIN 32525-4: 180 - 200 HB (as welded) 330 - 370 HB (work hardened)
- Service temperature: 300 C
- Weld deposit density: ~ 8 g/cc
- View Details →
- EN 14700 alloy category: Fe 11
- Available forms: welding electrodes, cored wires
- Major alloying elements: C ,Si, Cr, Ni, Mn, Fe
- Major hard-phase(s): -
- Hardness as per DIN 32525-4: 180 - 200 HB (as welded) 330 - 370 HB (work hardened)
- Service temperature: 300 C
- Weld deposit density: ~ 8 g/cc
- View Details →
- EN 14700 alloy category: Fe 11
- Available forms: welding electrodes, cored wires
- Major alloying elements: C ,Si, Cr, Ni, Mn, Fe
- Major hard-phase(s): -
- Hardness as per DIN 32525-4: 180 - 200 HB (as welded) 330 - 370 HB (work hardened)
- Service temperature: 300 C
- Weld deposit density: ~ 8 g/cc
- View Details →
- EN 14700 alloy category: Fe 11
- Available forms: welding electrodes
- Major alloying elements: C ,Si, Cr, Ni, Mn, Fe
- Major hard-phase(s): -
- Hardness as per DIN 32525-4: 180 - 200 HB (as welded) 330 - 370 HB (work hardened)
- Service temperature: 300 C
- Weld deposit density: ~ 8 g/cc
- View Details →
- EN 14700 alloy category: Fe 11
- Available forms: welding electrodes
- Major alloying elements: C, Si, Mn, Cr, Ni, Mo, Fe
- Major hard-phase(s): -
- Hardness as per DIN 32525-4: 180 - 200 HB (as welded) 330 - 370 HB (work hardened)
- Service temperature: From room temperature up to + 1200° C
- Weld deposit density: ~ 8 g/cc
- View Details →
- EN 14700 alloy category: Fe 11
- Available forms: welding electrodes
- Major alloying elements: C, Si, Mn, Cr, Ni, Mo, Fe
- Major hard-phase(s): -
- Hardness as per DIN 32525-4: 180 - 200 HB (as welded) 330 - 370 HB (work hardened)
- Service temperature: - 20° C up to +300° C
- Weld deposit density: ~ 8 g/cc
- View Details →
- EN 14700 alloy category: Fe 11
- Available forms: welding electrodes
- Major alloying elements: C, Si, Mn, Cr, Ni, Mo, Fe
- Major hard-phase(s): -
- Hardness as per DIN 32525-4: 180 - 200 HB (as welded) 330 - 370 HB (work hardened)
- Service temperature: - 60° C up to +300° C
- Weld deposit density: ~ 8 g/cc
- View Details →
- EN 14700 alloy category: Fe 12
- Available forms: welding electrodes
- Major alloying elements: C, Si, Cr, Ni, Mn, Fe
- Major hard-phase(s): -
- Hardness as per DIN 32525-4: -
- Service temperature: -120 °C up to +350 °C
- Weld deposit density: ~ 8 g/cc
- View Details →
- EN 14700 alloy category: Fe 10
- Available forms: welding electrodes, cored wires
- Major alloying elements: Cr, Ni, Mn, Fe
- Major hard-phase(s): None
- Hardness as per DIN 32525-4: 180 - 200 HB (as welded) | 400 - 500 HB (work hardened)
- Service temperature: 300 ᵒC
- Weld deposit density: ~ 8 g/cc
- View Details →