- Home
- Main Catalog
Hardcarb Products
Date (default)
Brands
Available forms
Hardness
Major hard-phase(s)
Suitability - Abrasion
Suitability - Corrosion
Suitability - Erosion
Suitability - Impact
Suitability - Temperature
- EN 14700 alloy category: EN 14700 E Fe 16
- Available forms: welding electrodes, cored wires
- Major alloying elements: C, Mn, Cr, Mo, Nb, V, W, Fe
- Major hard-phase(s): Chromium carbide, complex carbides
- Hardness as per DIN 32525-4: 65 - 68 HRC
- Service temperature: 800 C
- Weld deposit density: ~ 8.00 g/cc
- View Details →
- EN 14700 alloy category: Fe 16
- Available forms: welding electrodes, cored wires, composite wearplates
- Major alloying elements: C, Mn, Cr, Mo, Nb, V, W, Fe
- Major hard-phase(s): Chromium carbide, complex carbides
- Hardness as per DIN 32525-4: 63 - 66 HRC
- Service temperature: 750 C
- Weld deposit density: ~ 8.00 g/cc
- View Details →
- EN 14700 alloy category: Fe 16
- Available forms: welding electrodes, cored wires, composite wearplates
- Major alloying elements: C, Mn, Cr, Mo, Nb, V, W, Fe
- Major hard-phase(s): Chromium carbide, Complex carbides
- Hardness as per DIN 32525-4: 62 - 66 HRC
- Service temperature: 700 C
- Weld deposit density: ~ 8.00 g/cc
- View Details →
- EN 14700 alloy category: Z Fe 8
- Available forms: welding electrodes, cored wires
- Major alloying elements: C, Si, Mn, Cr, B, Fe
- Major hard-phase(s): Iron borides, chromium borides
- Hardness as per DIN 32525-4: 63 - 66 HRC
- Service temperature: 500 C
- Weld deposit density: ~ 8.00 g/cc
- View Details →
- EN 14700 alloy category: Fe 14
- Available forms: welding electrodes, cored wires, composite wearplates
- Major alloying elements: C, Mn, Mo, Ni, Cr, V, Nb, B, Fe
- Major hard-phase(s): Chromium carbide, Complex carbides
- Hardness as per DIN 32525-4: 61 - 65 HRC
- Service temperature: 600 C
- Weld deposit density: ~ 8.00 g/cc
- View Details →
- EN 14700 alloy category: Fe 14
- Available forms: welding electrodes, cored wires, composite wearplates
- Major alloying elements: C, Mn, Mo, Ni, Cr, V, Nb, B, Fe
- Major hard-phase(s): Chromium carbide, complex carbides
- Hardness as per DIN 32525-4: 62 - 66 HRC
- Service temperature: 600 C
- Weld deposit density: ~ 8.00 g/cc
- View Details →
- EN 14700 alloy category: Fe 14
- Available forms: welding electrodes, cored wires
- Major alloying elements: C, Mn, Cr, V, W, B, Fe
- Major hard-phase(s): Chromium carbide, Complex carbides
- Hardness as per DIN 32525-4: 60 - 65 HRC
- Service temperature: 550 C
- Weld deposit density: ~ 8.00 g/cc
- View Details →
- EN 14700 alloy category: Fe 14
- Available forms: welding electrodes, cored wires, composite wearplates
- Major alloying elements: C, Mn, Cr, Mo, Ni, Fe
- Major hard-phase(s): Chromium carbide
- Hardness as per DIN 32525-4: 58 - 62 HRC
- Service temperature: 550 C
- Weld deposit density: ~ 8.00 g/cc
- View Details →
- EN 14700 alloy category: Fe 16
- Available forms: welding electrodes, cored wires, composite wearplates
- Major alloying elements: C, Si, Mn, Cr, V, Fe
- Major hard-phase(s): Chromium carbide, Vanadium carbide
- Hardness as per DIN 32525-4: 62 - 66 HRC
- Service temperature: 500 C
- Weld deposit density: ~ 8.00 g/cc
- View Details →
- EN 14700 alloy category: Fe 16
- Available forms: welding electrodes, cored wires, composite wearplates
- Major alloying elements: C, Cr, Nb, Mo, W, V, B, Fe
- Major hard-phase(s): Chromium carbide, Complex carbide
- Hardness as per DIN 32525-4: 62 - 66 HRC
- Service temperature: 500 C
- Weld deposit density: ~ 8.00 g/cc
- View Details →
- EN 14700 alloy category: Fe 15
- Available forms: welding electrodes, cored wires, composite wearplates
- Major alloying elements: C, Si, Mn, Cr, Nb, B, Fe
- Major hard-phase(s): Chromium carbide, Complex carbide
- Hardness as per DIN 32525-4: 62 - 66 HRC
- Service temperature: 450 C
- Weld deposit density: ~ 8.00 g/cc
- View Details →
- EN 14700 alloy category: Fe 15
- Available forms: welding electrodes, cored wires, composite wearplates
- Major alloying elements: C, Si, Mn, Cr, Nb, B, Fe
- Major hard-phase(s): Chromium carbide, Complex carbide
- Hardness as per DIN 32525-4: 65 - 68 HRC
- Service temperature: 450 C
- Weld deposit density: ~ 8.00 g/cc
- View Details →