Care has to be taken that there is no contact between joint welding and hardfacing. This is mainly because most hardfacing deposits have 3-5% carbon, which will immediately cause the joint to crack. Alternatively, Nicrolloy 30/9 type of consumables can be used which do not allow carbon intake.